High strength and ductility in partially recrystallized Fe<sub>40</sub>Mn<sub>20</sub>Cr<sub>20</sub>Ni<sub>20</sub> high-entropy alloys at cryogenic temperature

Figure 10. Tensile deformation process of HEA annealed at 700 and 900 °C for 2 h. (A and B) Schematics of the microstructure of non-deformed sample. (C and D) Schematics of the microstructure of sample after fracture. HEA: High-entropy alloy.