fig11

Cryogenic atom probe tomography and its applications: a review

Figure 11. 3-D APT atom map and proximity histograms across the alkali-rich/alkali-poor interface in water and across the water/corroded glass interface. (A) 3-D APT atom map and proximity histograms across (B) the alkali-rich/alkali-poor interface in water and (C) across the water/corroded glass interface. Error bars indicate 1-sigma from standard counting error. Reproduced with the permission of Ref.[39] Copyright 2018, Elsevier.